coater
Specifications
|
Equipment speed |
Max5m/min |
|
Coating method |
Continuous coating/transfer gap coating |
|
Principal material |
Lithium cobaltate, ternary material, lithium iron phosphate, lithium manganate |
|
viscosity |
1500 ~ 30000cps |
|
Coating width |
100-300mm |
|
Single surface density range |
Positive electrode 100-300g/m2, negative electrode 100-250g/m2; |
|
Dry coating thickness |
50-200um |
|
Coating dry thickness error |
One side ±2μm; Both sides ±3μm (except edge, head and tail 8mm) |
|
Appearance requirement |
No wrinkles, no damage, no wave edge, no scratch, no crack, no bulge, no pollution |